| Nozzle: 240, Bed: 110
| Nozzle: 240, Bed: 110
| Nozzle: 240, Bed: 110
| Nozzle: 240, Bed: 110
| DO NOT use enclosed chamber. Weird, I know. Put a fan on it after the 1st layer. 1st layer may be wavy, you may have to slow down the 1st layer speed to like 15-20 mm/s (or maybe the bed's too hot??)     (╯⊙﹏⊙)╯︵ ┴─┴
| DO NOT use enclosed chamber. Weird, I know. Put a fan on it after the 1st layer. 1st layer may be wavy, you may have to slow down the 1st layer speed to like 15-20 mm/s, or perhaps maybe the bed's too hot??      (╯⊙﹏⊙)╯︵ ┴─┴
Thanks to Zach for suggesting not to use an enclosed chamber, it was driving me flipping insane.  
Thanks to Zach for suggesting not to use an enclosed chamber, it was driving me flipping insane.  
|-
|-