| Nov, 2018
| Hatchbox forest green ABS
| Nozzle: 240, Bed: 110
| Nozzle: 240, Bed: 110
| DO NOT use enclosed chamber, weird I know. Put a fan on it after the 1st layer. 1st layer may be wavy, you may have to slow down the 1st layer a lot (like 15-20 mm/s).
|-
| Nov, 2018
| AMZ3D Black, ABS
| Nozzle: 235, Bed: 110
| Nozzle: 230, Bed: 110
| Use enclosed chamber. Settings still not tweaked precisely, may over-extrude. Try lowering the temp by 5 deg, or set extrusion to 0.95
|-
|-