| Nozzle: 240, Bed: 110 | | Nozzle: 240, Bed: 110 | ||
| Nozzle: 240, Bed: 110 | | Nozzle: 240, Bed: 110 | ||
| DO NOT use enclosed chamber, weird I know. Put a fan on it after the 1st layer. 1st layer may be wavy, you may have to slow down the 1st layer a lot (like 15-20 mm/s). | | DO NOT use enclosed chamber, weird I know. Put a fan on it after the 1st layer. 1st layer may be wavy, you may have to slow down the 1st layer a lot (like 15-20 mm/s). Thanks to Zach for suggesting not to use an enclosed chamber, it was driving me flipping insane. | ||
|- | |- | ||