Line 18: Line 18:
* Retraction Enabled
* Retraction Enabled
** Z Hop when Retracting: 0.5mm (NO Z Hop used with PLA)
** Z Hop when Retracting: 0.5mm (NO Z Hop used with PLA)
* Print Speed: 30mm/s (Down from 60mm/s for PLA)
* Print Speed: 25mm/s (Down from 60mm/s for PLA)
* Pringing Temp.: 230°C
* Pringing Temp.: 235°C
* Filament Diameter: whatever a micrometer reads for this reel.
* Filament Diameter: whatever a micrometer reads for this reel.
* Flow: 80%
* Flow: 65%
* Nozzle Size: 0.4mm
* Nozzle Size: 0.4mm
Advanced Tab:
Advanced Tab:
* Retraction Distance: 3.5mm (Down from 4.5mm for PLA)
* Retraction Speed: 30.0mm/s
* Travel Speed: 250mm/s (Up from 150mm/s for PLA)
* Retraction Distance: 0.3mm
* Travel Speed: 250mm/s
* Bottom Layer Speed: 20mm/s
* Infill Speed: 30mm/s
* Outer Shell Speed: 20mm/s
NOTES:
* The above settings are a "best compromise", to get '''good''' results, without limiting the print speed any more than necessary.
* Check the print head periodically. If PETG is building up on that, touch with a Q-tip (while printing) to wick the plastic off. (Before it drops as a blob onto the print.)